A cryogenic XPS study of Ce fixation on nanosized manganite and vernadite: Interfacial reactions and effects of fulvic acid complexation
Umeå universitet, Teknisk-naturvetenskapliga fakulteten, Kemiska institutionen.
Umeå universitet, Teknisk-naturvetenskapliga fakulteten, Kemiska institutionen.
Visa övriga samt affilieringar
2018 (Engelska)Ingår i: Chemical Geology, ISSN 0009-2541, E-ISSN 1872-6836, Vol. 483, s. 304-311Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

This study investigated interfacial reactions between aqueous Ce(III) and two synthetic nanosized Mn (hydr-) oxides (manganite: gamma-MnOOH, and vernadite: delta-MnO2) in the absence and presence of Nordic Lake fulvic acid (NLFA) at circumneutral pH by batch experiments and cryogenic X-ray photoelectron spectroscopy (XPS). The surfaces of manganite and vernadite were negatively charged (XPS-derived loadings of (Na+ K)/Cl > 1) and loaded with 0.42-4.33 Ce ions nm(-2). Manganite stabilized Ce-oxidation states almost identical to those for vernadite (approximately 75% Ce(IV) and 25% Ce(III)), providing the first experimental evidence that also a Mn (III) phase (manganite) can act as an important scavenger for Ce(IV) and thus, contribute to the decoupling of Ce from its neighboring rare earth elements and the development of Ce anomaly. In contrast, when exposed to Ce (III)-NLFA complexes, the oxidation of Ce by these two Mn (hydr-) oxides was strongly suppressed, suggesting that the formation of Ce(III) complexes with fulvic acid can stabilize Ce(III) even in the presence of oxidative Mn-oxide surfaces. The experiments also showed that Ce(III) complexed with excess NLFA was nearly completely removed, pointing to a strong preferential sorption of Ce(III)-complexed NLFA over free NLFA. This finding suggests that the Ce(III)-NLFA complexes were most likely sorbed by their cation side, i.e. Ce(III) bridging between oxide groups on the Mn (hydr-) oxides and negatively-charged functional groups in NLFA. Hence, Ce(III) was in direct contact with the oxidative manganite and vernadite but despite that not oxidized. An implication is that in organic-rich environments there may be an absence of Ce(IV) and Ce anomaly despite otherwise favorable conditions for Ce(III) oxidation.

Ort, förlag, år, upplaga, sidor
Elsevier, 2018. Vol. 483, s. 304-311
Nyckelord [en]
Cryogenic XPS, Manganite, Vernadite, Oxidative scavenging, Ce anomaly
Nationell ämneskategori
Fysikalisk kemi
Identifikatorer
URN: urn:nbn:se:umu:diva-138591DOI: 10.1016/j.chemgeo.2018.02.033ISI: 000429492300027OAI: oai:DiVA.org:umu-138591DiVA, id: diva2:2903
Forskningsfinansiär
Vetenskapsrådet, 2016-03808Vetenskapsrådet, 2016-03808Forskningsrådet Formas, 2017-00766Tillgänglig från: 2018-06-26 Skapad: 2018-06-26 Senast uppdaterad: 2018-06-26Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltext

Sök vidare i DiVA

Av författaren/redaktören
Yu, ChangxunBoily, Jean-FrancoisShchukarev, Andrey
Av organisationen
Kemiska institutionen
I samma tidskrift
Chemical Geology
Fysikalisk kemi

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 542 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • Vancouver
  • biomed-central
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf